INTRODUCTIO
Donboiler212 polyether mixtio polyoliorum constat ex polyolis, catalysto, agente flatu et aliis additivis.Potest cum isocyanate agere, ut polyurethanum spumam rigidam formet cum proprietate optimae scelerisque velit.
TYPICA PROPRIETAS
Aspectus | Brown-flavus viscosus liquor perspicuus |
Hydroxyl valorem mgKOH/g | 300-400 |
Viscositas 25℃ , mPa·s | 300-500 |
Densitas 20℃ , g/cm3 | 1.05-1.15 |
RECOMMENDED RATIO
pbw * | |
Donboiler 212 mixtura polyol | 100 |
Isocyanate | 120±5 |
Materia temperatus | 22±2 |
REACTION CARACTERES
Manual Mixing | Princeps Pressura Machina Mixing | |
Crepito Tempus s | 10±2 | 7±2 |
Gel tempus s | 55±3 | 40-50 |
Convertendi cursum otium s | 70-90 | 50-70 |
Free densitas kg/m3 | 26.5-27.5 | 25.5-27 |
PLAGA PERFUNCTIONES
Density CUMATIUM | Kg/m3 | ≥35 |
Clausa-cellula rate | % | ≥95 |
Scelerisque Conductivity (10℃) | W/mk | ≤0.02 |
Compressive vires | KPa | ≥120 |
Dimensionalis stabilitas 24h -30℃ | % | ≤0.5 |
24h 100℃ | % | ≤0.5 |
FASCICULUS
220kg/orum vel 1000kg/IBC, 20000kg/flexi piscina vel ISO Tank.