Donfoam 901 amanzi base benld polyols ukuthululwa
Donfoam 901 amanzi base benld polyols ukuthululwa
ISINGENISO
Lo mkhiqizo uwuhlobo lwenhlanganisela ye-polyols namanzi angu-100% njenge-ejenti evuthelayo, ecwaningwa ngokukhethekile nge-PUF eqinile.Izici zimi kanje:
(1) ukugeleza okuhle, Ifanele ukuthululwa ngesikhathi esisodwa.
(2) izici ezinhle kakhulu zemishini yegwebu
(3) izinga lokushisa eliphakeme kakhulu lokuzinza kobukhulu obuphezulu/eliphansi
IMPAHLA YOMNYAMA
Ukubukeka | Uketshezi olusobala olukhanyayo oluphuzi kuya kokunsundu |
Inani le-Hydroxyl mgKOH/g | 300-400 |
I-Viscosity 25℃ , mPa·s | 1800-2400 |
Ukuminyana 20℃ , g/cm3 | 1.00-1.10 |
Izinga lokushisa lesitoreji | 10-25 |
Inyanga yokuzinza kwesitoreji | 6 |
UBUCHWEPHESHE KANYE NEZIPHUMA ZOKUSEBENZA
Izinga lokushisa lesici lingu-20 ℃, inani langempela liyahlukahluka kuye ngokuthi ububanzi bepayipi kanye nesimo sokucubungula.
Ukuxuba ngezandla | Umshini wokucindezela okuphezulu | |
Isilinganiso (POL/ISO) g/g | 1:1.0-1.1.20 | 1:1.0-1.20 |
Isikhathi sokukhuphuka s | 60-90 | 40-70 |
Isikhathi se-gel s | 200-240 | 150-200 |
Thatha isikhathi samahhala s | ≥300 | ≥260 |
I-Core Free density kg/m3 | 60-70 | 60-70 |
Isilinganiso (POL/ISO) g/g | 1:1.0-1.1.20 | 1:1.0-1.20 |
IMISEBENZI YEgwebu
Ukuminyana kwegwebu | I-GB/T6343-2009 | 60~80kg/m3 |
Amandla Acindezelayo | I-GB/T8813-2008 | ≥480KPa |
Izinga leseli elivaliwe | I-GB 10799 | ≥95% |
I-Thermal conductivity (15℃) | GB 3399 | ≤0.032mW/(mK) |
Ukumuncwa kwamanzi | I-GB 8810 | ≤3(V/V) |
Ukumelana nokushisa okuphezulu |
| 140 ℃ |
Ukumelana nezinga lokushisa eliphansi |
| -60 ℃ |
IPHAKETHI
220kg/drum noma 1000kg/IBC, 20,000kg/flexi tank noma ISO Tank.