Polyester-based TPU-Hotmelt Film
Ukuqina: Unxweme A 70 – Unxweme A 97
Iimpawu: Ukunamathela okulungileyo kwi-TPU, inayiloni, i-PVC, ilaphu, isikhumba kunye nezinye izinto, kwaye emva kokudibana, ineempawu zokuqina okuphezulu, ukuqina okuphezulu, ukuxhathisa ukunxiba kunye nokunwebeka okulungileyo.
Usetyenziso: Ifilimu ekwiKhalenda, umgubo ocoliweyo, ifilimu eNgafihliyo, ilaphu lokwanyisa, izixhobo zesihlangu, iiteyiphu zokutywina ze-Seam njl.
Izinto |
Ukuqina | Tensile strength |
Sindawo yokukholisa |
MeltFphantsiRwatya | LaminatingTi-emperature | Tack Free Time |
Umgangatho | I-ASTM D2240 | I-ASTM D412 | I-ASTM D36 | I-ASTM D1238 | Indlela ye-INOV | Indlela ye-INOV |
Iyunithi | Unxweme A | MPa | ℃ | g/10min | ℃ | imiz |
T5160 | 97 | 18 | 75 | 33-36 | 70-80 | 3 |
T5260 | 97 | 20 | 80 | 16-18 | 75-85 | 3.5 |
T5260H | 97 | 23 | 85 | 11-13 | 80-90 | 4 |
T6195 | 97 | 25 | 130 | 20-25 | 110-140 | 10 |
T6185 | 97 | 28 | 140 | 15-20 | 120-150 | 12 |
Izinto |
Ukuqina | Tensile strength | Ukwandisa |
Flow IsiqaloTi-emperature |
Sindawo yokukholisa | LaminatingTi-emperature |
Umgangatho | I-ASTM D2240 | I-ASTM D412 | I-ASTM D412 | Indlela ye-INOV | I-ASTM D36 | Indlela ye-INOV |
Iyunithi | Unxweme A | MPa | % | ℃ | ℃ | ℃ |
B480 | 81 | 16 | 800 | 95 | 115 | 120-140 |
B485 | 85 | 18 | 950 | 103 | 125 | 130-150 |
T5170 | 72 | 18 | 850 | 105 | 126 | 130-150 |
T5170-1 | 72 | 18 | 850 | 105 | 126 | 100-150 |
T5175 | 77 | 19 | 800 | 113 | 133 | 140-160 |
T5175-1 | 77 | 19 | 800 | 113 | 133 | 110-160 |
T5185-10 | 82 | 24 | 850 | 122 | 146 | 140-160 |
T5185-9 | 82 | 24 | 850 | 122 | 146 | 120-170 |
T5190 | 91 | 19 | 750 | 115 | 133 | 140-160 |