Polikaprolakton tipidagi prepolimer
Qattiqlik; qirg'oq A 60A - qirg'oq A 95A
Mahsulot yaxshi ishlash, keng qattiqlik diapazoni, yaxshi xususiyatlarga ega
Model | D4336 | D4142 | D4152 | D4160 |
NCO/% | 3,6±0,2 | 4,2±0,2 | 5,2±0,2 | 6,0±0,2 |
20 ℃ holatida | Och sariq rangli qattiq | |||
MOKA100 g Prepolimer / g | 10.5 | 12 | 14.9 | 17.5 |
Aralash harorati /℃(Prepolimer /MOCA) | 80/120 | 80/120 | 80/120 | 80/120 |
Jel vaqti / min | 8 | 8 | 7.5 | 4 |
Vulkanizatsiyadan keyingi vaqt (100 ℃) / soat | 16 | 16 | 16 | 16 |
Qattiqlik (Shore A) | 80±2 | 88±2 | 92±2 | 94±2 |
100% modul/MPa | 3.3 | 5.4 | 7.3 | 10.5 |
300% modul / MPa | 6.1 | 10.6 | 15.6 | 18.7 |
Kuchlanish kuchi / MPa | 45 | 45 | 50 | 52 |
Cho'zilish / % | 550 | 520 | 480 | 450 |
Yırtilish kuchi / (KN / m) | 51 | 76 | 99 | 110 |




Xabaringizni shu yerga yozing va bizga yuboring