The hardness of the product can be adjusted by adjusting the ratio of a / b material. The product is colorless and transparent, has good viscosity, elongation at break and good yellowing resistance.
Component B |
model |
DX1610–B |
appearance |
Colorless transparent liquid |
|
Component A |
model |
DX1615-A |
appearance |
Colorless transparent liquid |
|
Ratio A:B(quality) |
100:22~25 |
|
Operating temperature /℃ |
30~40 |
|
Gel time(30℃)*/min |
2~3min |
|
Properties of finished rubber |
||
appearance |
Colorless transparent elastomer |
|
Hardness(shore C) |
20~40 |
|
tensile strength /MPa |
2 |
|
Elongation / % |
800~1000 |
|
Density/(g/cm3) |
1.05 |
The production process is simple and suitable for assembly line production. The product is transparent in color and has good wear resistance and resilience.
Cushion |
model |
DS1600-A |
DS1640-B |
appearance |
Clear near water-white liquid |
Clear near water-white liquid |
|
Ratio A:B(quality) |
100:30 |
||
Operating temperature /℃ |
25~40 |
25~40 |
|
Gel time(70℃)*/min |
1-4 |
||
appearance |
Colorless or light yellow colloidal solid |
||
Hardness(shore A) |
0-2 |
||
Hard pad |
model |
DS1670-A |
DS1622-B |
appearance |
Color or light yellow liquid |
Clear near water-white liquid |
|
Ratio A:B(quality) |
100:40~45 |
||
Operating temperature /℃ |
25~40 |
25~40 |
|
Gel time(70℃)*/min |
1-4 |
||
appearance |
Colorless or light yellow transparent elastomer |
||
Hardness(shore A) |
65±5 |