MDI Prepolymer
dite: rivaj A 75A - rivaj A 95A
Pwodwi a gen karakteristik sa yo nan bon rezistans mete, detèminasyon ak ekselan pwopriyete mekanik.
Itilize pou fè divès kalite pwodwi elastomè an poliyiretàn tankou wou kawotchou, plak Van ak bag sele.
Modèl
| D2560 | D2575 | D2590 | D3565 | D3575 | D3590 |
NCO/% | 6.0±0.2 | 7.5±0.2 | 9.0±0.2 | 6.5±0.2 | 7.5±0.2 | 9.0±0.2 |
Eta a 20 ℃ | Sistèm PTMG, blan solid | Sistèm Polyester, solid blan | ||||
BDO100g Prepolymer /g | 6.1 | 7.8 | 9.3 | 6.8 | 7.8 | 9.3 |
Viskozite (85℃)/mPa·s | 1400 | 1000 | 750 | 1400 | 1200 | 1000 |
Tanperati melanje /℃(Prepolymer /1,4BD) | 80/40 | 80/40 | 80/40 | 80/40 | 80/40 | 80/40 |
Tan jèl / min | 10 | 8 | 7 | 10 | 8 | 7 |
Apre tan vulkanizasyon (110 ℃) / h | 48 | 48 | 48 | 48 | 48 | 48 |
Dite (Shore A) | 87±2 | 90±2 | 95±2 | 85±2 | 90±2 | 95±2 |
100% Modil / MPa | 6 | 9.2 | 12.6 | 5 | 8.6 | 12.3 |
300% Modil / MPa | 17 | 16.6 | 18.9 | 10 | 19.7 | 29.1 |
Fòs rupture / MPa | 44 | 43 | 45 | 50 | 46 | 55 |
elongasyon / % | 472 | 683 | 500 | 540 | 580 | 530 |
Fòs chire / (KN/m) | 75 | 110 | 130 | 82 | 117 | 132 |
Rebondisman / % | 61 | 64 | 55 | 43 | 35 | 39 |
Dansite (24℃)/(g/cm3) | 1.11 | 1.11 | 1.12 | 1.23 | 1.26 | 1.24 |
Din mete / mm³ | 36 | 44 | 44 | 32 | 35 | 38 |
Ekri mesaj ou a isit la epi voye li ba nou