Mdi prepolymer
Caledwch : Traeth A 75A - Traeth A 95A
Mae gan y cynnyrch nodweddion ymwrthedd gwisgo da, gwytnwch ac eiddo mecanyddol rhagorol.
Fe'i defnyddir i wneud cynhyrchion elastomer polywrethan amrywiol fel olwynion rwber, platiau rhidyll a modrwyau selio.
Fodelith
| D2560 | D2575 | D2590 | D3565 | D3575 | D3590 |
NCO/% | 6.0 ± 0.2 | 7.5 ± 0.2 | 9.0 ± 0.2 | 6.5 ± 0.2 | 7.5 ± 0.2 | 9.0 ± 0.2 |
Nodwch yn 20 ℃ | System PTMG, solid gwyn | System Polyester, Solid Gwyn | ||||
BDO100g prepolymer /g | 6.1 | 7.8 | 9.3 | 6.8 | 7.8 | 9.3 |
Gludedd (85 ℃)/mpa · s | 1400 | 1000 | 750 | 1400 | 1200 | 1000 |
Tymheredd Cymysgu /℃ (prepolymer /1,4bd) | 80/40 | 80/40 | 80/40 | 80/40 | 80/40 | 80/40 |
Amser Gel /Min | 10 | 8 | 7 | 10 | 8 | 7 |
Amser ôl -fulcanization (110 ℃)/h | 48 | 48 | 48 | 48 | 48 | 48 |
Caledwch (lan a) | 87 ± 2 | 90 ± 2 | 95 ± 2 | 85 ± 2 | 90 ± 2 | 95 ± 2 |
Modwlws/MPA 100% | 6 | 9.2 | 12.6 | 5 | 8.6 | 12.3 |
Modwlws /MPA 300% | 17 | 16.6 | 18.9 | 10 | 19.7 | 29.1 |
Cryfder tynnol /mpa | 44 | 43 | 45 | 50 | 46 | 55 |
Elongation / % | 472 | 683 | 500 | 540 | 580 | 530 |
Cryfder rhwygo /(kn /m) | 75 | 110 | 130 | 82 | 117 | 132 |
Adlam / % | 61 | 64 | 55 | 43 | 35 | 39 |
Dwysedd (24 ℃)/ (g/ cm3) | 1.11 | 1.11 | 1.12 | 1.23 | 1.26 | 1.24 |
Gwisgo din /mm³ | 36 | 44 | 44 | 32 | 35 | 38 |




Ysgrifennwch eich neges yma a'i hanfon atom